Friday, March 10, 2017

Re: [MW:26185] Can we use E 309L consumable for joining of A105 vlave+ 316Ti pipe?

309L is used dor ss to ms

On 8 Mar 2017 2:07 p.m., "'Sankaran Sp' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Dear friends,

Can you clarify the following points?

we are planning to welding of nipple(pipe) of A 269 TP 316Ti pipe with A105 forged steel valve, welding is socket weld( fillet ) only. while welding of these combination can we use Er 309L type consumable? or any Ti added consumable to be used? 
no specific requirement from customer, kindly clarify and do the needful.

Regards,

Sankaran.sp 
welding& metallurgy expert 
coimbatore, india.     

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/142944870.1439859.1488967175410%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK8EmDROVoTkbP3YrN%3D3Ohidu3NYtE3zQFMnE5nXM9NeaQ6rJA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...