Re: [MW:26142] Shell life

Dear pls,

go with API 653


*DINESH VITTHAL SOMWANSHI*

*BACHELOR IN MECHANICAL ENGINEER*

*AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL,*
*API 570 - Piping Inspector,** AWS - CWI , CSWIP 3.1*,*BGAS  Gr 2 / 3*
*NDT II -UT , RT , MT , PT, VT*
00919881344135
Skype = dinesh570_1

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*


On Tue, Feb 28, 2017 at 7:49 PM, Narasimha Rao <narasimharao.kaja@gmail.com> wrote:

Dear friends,
         Can anyone tell us formula for tank shell plate life calculation.
Shell plate thickness initial 20mm
shell plate thickness after 15 years 19mm. Corrosion allowance 1.5 mm.

KVN Rao

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGJWGdN7P8fw4%2BFyt-uo5G7zsCcV0YNxnav1L5%2BCxphT3xEu-g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrWW1y4eNRokROudJLLzTV8iFi_8m5hw2awB79YryoXCHQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...