Shell has some imp aspects & components like Design considerations & requirements, plate arrangements, joints, compression at joint at she'll n roof, & at btm, nozzles, 80+mm nozzles, wldg of she'll btm, upper n lower she'lls.
u may elaborate specific requirements
Chandrakant Mohikar (ex. PDO, Area Project QA )
On 1 Mar 2017 08:10, "Narasimha Rao" <narasimharao.kaja@gmail.com> wrote:
-- Dear friends,
Can anyone tell us formula for tank shell plate life calculation.
Shell plate thickness initial 20mm
shell plate thickness after 15 years 19mm. Corrosion allowance 1.5 mm.KVN Rao
--
http://www.linkedin.com/groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
To post to this group, send email to materials-welding@googlegroups.com .
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ CAGJWGdN7P8fw4%2BFyt- uo5G7zsCcV0YNxnav1L5% 2BCxphT3xEu-g%40mail.gmail.com .
For more options, visit https://groups.google.com/d/optout .
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE4dwYMc%3Dow%3DhbVQ_NyQYdeQEVvMan7hVjjTK3aR_i95GzELCw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments