Re: [MW:25990] ERCoCr-A hardfacing Overlay on SS410

Dear friend,

ERCoCr-A can be hard faced as overlay on A217-CA15 type cast material by GTAW process, which is equivalent to  A276 410 composition, since A276- 410 is bar material and no code is allowed to hard face or deposit on these type of bar material.  
 
 PWHT can be followed as per ASME sec VIII div 1 standard with reference to Pno :6 ,time &  temperature also avilable.
 
regards.
sankaran.sp
welding& metallurgy specialist


On Wednesday, 25 January 2017 2:21 PM, Brajendra Singh <brajendrasingh523@gmail.com> wrote:


Dear Experts,
 
Need your opinion  for ERCoCr-A hard facing overlay on A276 410 ( with 2.5mm finished overlay thickness) by GTAW Welding Process.
 
1. What weld parameters required for welding.
2. PWHT requirement (time &  temperature required).
 
Qualification standard is ASME Sec IX.

Thanks in advance


Thanks & Regards,
Brajendra  S. Patel
Pune, India
cont:+917057406907

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA9DSA-fgn_AkjsxgJ08B0MD%3DiH%2BC3DxbzVGA2sHXWSysmyrgw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...