Thursday, January 26, 2017

Re: [MW:25987] WELD DISTANCE AS PER ASME-

Please let me know reference STD no.

Sikhandar

On Wed, Jan 25, 2017 at 4:08 PM, cd murali <cdmurali09@gmail.com> wrote:
The minimum distance between parallel butt welds shall be 20 mm or three times the wall thickness of the joint, whichever is greater as per Saudi Aramco Standard

Regards


C.D.Mural
i
 
| QA/QC 
​Welding/Piping Inspector
| M.S. Al-Suwaidi Industrial Services Company Ltd| Rabigh Phase-II Petrochemical Project (G.S.T), AR-4501|




On Sat, Dec 10, 2016 at 6:28 AM, Raneesh.PK <pkraneesh@gmail.com> wrote:
Dear experts,

Can any one please confirm the Minimum distance between butt weld joint as per ASME B31.1.

Regards,


RANEESH.PK

QA/QC-WELDING


BEC

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGRQ%2BmXZ3%3DqAKgPuTe8UsghXfEdiwt1A11WWZQeYoJqhK%3D0TSg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BpoiyA-b494qvkOq2Z0POH%2BJqYCLBf%3D_KbkqcYkVnD-YquNgw%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPGmqAMTXLpYTsf279x7qtnxKAThd0qS6MhiMrC1_MjGW%3D-05w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...