Thursday, January 26, 2017

Re: [MW:25986] WELD DISTANCE AS PER ASME-

There is no limitation on B31.1
There is a limitation in PCC-2 but this is applicable for repairs

2017-01-26 9:15 GMT+02:00 Kannayeram Gnanapandithan <kgpandithan@gmail.com>:

Weld toe to toe is around ,13mm


On 26-Jan-2017 12:12 pm, "cd murali" <cdmurali09@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (cdmurali09@gmail.com) Add cleanup rule | More info

The minimum distance between parallel butt welds shall be 20 mm or three times the wall thickness of the joint, whichever is greater as per Saudi Aramco Standard

Regards


C.D.Mural
i
 
| QA/QC 
​Welding/Piping Inspector
| M.S. Al-Suwaidi Industrial Services Company Ltd| Rabigh Phase-II Petrochemical Project (G.S.T), AR-4501|




On Sat, Dec 10, 2016 at 6:28 AM, Raneesh.PK <pkraneesh@gmail.com> wrote:
Dear experts,

Can any one please confirm the Minimum distance between butt weld joint as per ASME B31.1.

Regards,


RANEESH.PK

QA/QC-WELDING


BEC

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGRQ%2BmXZ3%3DqAKgPuTe8UsghXfEdiwt1A11WWZQeYoJqhK%3D0TSg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BpoiyA-b494qvkOq2Z0POH%2BJqYCLBf%3D_KbkqcYkVnD-YquNgw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOPTn19pDnzKOf67uqGcMSuf5%2B5ASwA7Ew3DcRDaECyvA%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40ALSYb_GbpGjNGbP%2Bq%2B7zQevsTQVJ3FCgXc_Rde8j0CpQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...