Re: [MW:25956] Fillet size a6 with single layer (GMAW welding process)

Use 1.6mm, amp around 355


On 16-Jan-2017 10:12 am, "Vijay Katkar" <katkar.vijay22@gmail.com> wrote:
Dear Experts,

Our customer is forcing us to do multilayer welding for 6mm throat size, which is increasing our welding time because most of welding is in a6 size.

I have tried so many test coupon to prove that a6 can be done by single layer but I am not succeed in all test.

Customer requirement is root penetration at least 0.3 mm. But I am not able to achieve it. refer following parameters which I have used.

  • Welding process :- GMAW
  • Filler Wire :- ER 70 S6 (1.2 mm dia)
  • Shielding gas :- 80 % Argon + 20 % Co2
  • Current :- 245-255 Amp
  • Voltage :- 26.5 to 27.5
  • Travel speed :- 220 - 240 mm/min
Please advise any modification is required in the parameters.  

Should I change Shielding gas composition?

Waiting for your valuable reply?

Thank you

Vijay Katkar

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP37wrKnxUoYE9r4ACS5vgf2Yo1UWw3MqJD25Khyw9LJDMG1Tw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNnuo8h7GBukApQOm-porkj8PRk%2BMeJYg6sSrALXSqSaA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...