Re: [MW:25940] Sec. IX- QW-403.5

If impact test is not required by the design and manufacturing Code Section then it is OK



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Unni Romes <unniromes@gmail.com>
Date: 18/01/2017 13:41 (GMT+02:00)
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25924] Sec. IX- QW-403.5

Dear all,

Please be clarified, 

SMAW, PQR is qualified with P1, G1 to P1, G1, 

as group number is supplimentary, 

Does this PQR support the WPS for P1 G1 to P1 G2

Is there any interpretation reference for this? 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a1a6fa46-8cc1-41c7-ade8-f0f0f5a8bc33%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...