Wednesday, January 18, 2017

Re: [MW:25932] Combining 2 PQRS

Check qualification limit for dia as per Sec IX.

On Jan 17, 2017 6:00 PM, "Lalit Malla" <lalit.malla@gmail.com> wrote:
Dear Expert,

I am having 2 PQRs i.e.:
1. 2" Sch. 80 Pipe (thk.-5.54mm) - GTAW (70S-2)
2. 6" Sch. 160 Pipe (thk.-18.26mm) - SMAW (7018)

My question is: Can I combine these 2 PQRs for buiding up one more making new WPS for 8" Sch. 80 Pipe (thk.-12.70mm) using GTAW+SMAW (Root and hot with GTAW and filling and capping with SMAW)

Thanx in advance

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c48bcc22-b50c-4d5a-8147-e4a0c3a3db39%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFw%3DPEhga7Jo%2BWUMOgq5bcSw-K%2BTPfVvdCj7_sAGqib8X5aLPQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...