Wednesday, January 18, 2017

RE: [MW:25924] Combining 2 PQRS

Yes u can pls.refer sec Ix welding general requirement.

On 17 Jan 2017 9:35 pm, "John Henning" <jhenning@deltak.com> wrote:

NO - Per ASME IX.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Lalit Malla
Sent: Tuesday, January 17, 2017 6:07 AM
To: Materials & Welding
Subject: [MW:25915] Combining 2 PQRS

 

Dear Expert,

 

I am having 2 PQRs i.e.:

1. 2" Sch. 80 Pipe (thk.-5.54mm) - GTAW (70S-2)

2. 6" Sch. 160 Pipe (thk.-18.26mm) - SMAW (7018)

 

My question is: Can I combine these 2 PQRs for buiding up one more making new WPS for 8" Sch. 80 Pipe (thk.-12.70mm) using GTAW+SMAW (Root and hot with GTAW and filling and capping with SMAW)

 

Thanx in advance

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c48bcc22-b50c-4d5a-8147-e4a0c3a3db39%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/MWHPR03MB28167C7A015E4BD1CA3AEB91A17C0%40MWHPR03MB2816.namprd03.prod.outlook.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPkJdRKm7zjORZR5%2BbquvLEO%3DV%2BWOmGNBqWNTZt2dgMXV0TTMA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...