Dear Raneesh,

The distance between adjacent butt welds is 1D. If not it is never closer than 1 1/2" . This is supposedly to prevent the overlap of HAZs. Min. Spacing of circumferential welds between centerlines shall not be less than 4 times the pipe wall thickness or 25 mm which ever is greater.

On Jan 17, 2017 2:28 PM, "George Dilintas" <dilintas@gmail.com> wrote:
tHERE IS NO RESTRICTION IN THIS CODE SECTION.
HOWEVER, YOU HAVE TO CONSIDER METALLURGICAL ISSUES.
ONCE MORE, CODE IS NOT AN ENGINEERING HANDBOOK

2017-01-13 9:00 GMT+02:00 syahrul husin <syahrulhisyam89@gmail.com>:


Dear Raneesh,

i m not an expert.But i m sure the allowable distance between the weld would be 4T or 50mm.




On Saturday, December 10, 2016 at 11:35:45 AM UTC+8, raneesh pk wrote:
Dear experts,

Can any one please confirm the Minimum distance between butt weld joint as per ASME B31.1.

Regards,


RANEESH.PK

QA/QC-WELDING


BEC

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ced9223d-c87f-487d-a6fe-764bb18aff69%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40B46fUjZPQu1Ec8Y1pz-e5beSjAW1kD%3DUN%2Bs%3DF7Kt2ULA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO4WkWkzWpUxvgcKvEh4EHC7%2B7LvmXAnGtkBuo2L3ATaJFchSg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...