Thanks sir,
                     I appreciate your guidance... my doubt is If he weld the lower thickness with the same parameters then what will be happened...? Is any impacts in mechanical properties? Please explain...!

Thanks and regards,

Krishnasamy. M

Sent from my iPhone

On Dec 27, 2016, at 5:09 PM, joydev dalai <joykolkata07@gmail.com> wrote:

Dear Krishnasamy,

As per API 1104 Thickness range is a essential variable for WQT. Please go through the Cl. No- 6.2.2 ( Scope) Point - e
for your reference  

On Tue, Dec 27, 2016 at 11:31 AM, Krishnasamy Masanam <krishnasamy1968@gmail.com> wrote:
Dear Experts,
Have a nice day to you all... I have doubt about welder qualification thickness range.

One of the welder has been successfully completed his WQT as per API 1104 with the thickness 21.1mm followed by the the 21.1 to 31.935mm thickness range WPS. Is he eligible for below 4.8 to 19.mm (0.188" to 0.750") if he cannot weld the lower thickness, why?

In API 1104, thickness is essential variable

I am expecting a favorable reply... thanks in advance...

Krishnasamy. M

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAETCo_rCwfu7KdBxGQUhhA5QiSHC-ZSa%3DLMkkyUUO2ZpRSzQdg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--



Best Regards,

Joydev Dalai
Dy. Manager - QA/QC
+91-7260898902
JHPL Project,
Kalpataru Power Transmission ltd.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFQz-VK7aDtmO0bThBbDtqwYN5dvdqba-X1N5EQz7MH36weJiA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .