Re: [MW:25798] For Cryogenic Services at Temp -196 degree Celsius (17 Kelvin) Pipe of ASTM 312 TP 304 L is suitable?

Hi

You can select 316L for this cryogenic application.
I have used it in various projects in past.

Regards

Prem Nautiyal 
9769316004




Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: vivek singh Chaudhary <viveksinghme1612@gmail.com>
Date: 05/12/2016 23:02 (GMT+05:30)
To: materials-welding@googlegroups.com
Subject: [MW:25795] For Cryogenic Services at Temp -196 degree Celsius (17 Kelvin) Pipe of ASTM 312 TP 304 L is suitable?

Dear Experts,

Currently I am working on a project of ISRO (Indian Space Research Organisation) for Integrated Cryogenic Engine Testing Facility (ICET), for bidding in that services are Liquid Hydrogen, Liquid Oxygen, Liquid Helium, Liquid Nitrogen, Gaseous Hydrogen, Gaseous Oxygen, Gaseous Nitrogen, Gaseous Helium.

For SS Seamless Pipes client has given three options for material ASTM 312 TP 304L/ ASTM 312TP 316L/ ASTM 312TP 321. 

Kindly suggest me the suitable material for the same that gives economical and best design.


Thanks in advance.


Regards:-

Vivek Singh Chaudhary

Piping Design Engineer.

Contact No.- +91 9990441755.

Email :- viveksinghme1612@gmail.com



--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP6FfyH8HRZ%3Dk7QQbBvHyjqSCXryhuoGtrw%2BHJ4_aKcSrp0fHg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...