Re: [MW:25818] For Cryogenic Services at Temp -196 degree Celsius (17 Kelvin) Pipe of ASTM 312 TP 304 L is suitable?

Hi,

ASTM 312 TP304L Suitable base on my experience, currently im involved with LNG TANK EPCC,all the pipe work we use 304L.


On Wednesday, December 14, 2016 3:17 PM, dilintas <dilintas@gmail.com> wrote:


They are more difficult to weld tham austenitic ss but cheaper. 304 and 316 are more reliable



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: 'Shashank Vagal' via Materials & Welding <materials-welding@googlegroups.com>
Date: 06/12/2016 07:04 (GMT+02:00)
To: materials-welding@googlegroups.com
Cc: Samarth Vagal <samarth.vagal@gmail.com>, Nachiket Vagal <nachi.vagal@gmail.com>
Subject: Re: [MW:25799] For Cryogenic Services at Temp -196 degree Celsius (17 Kelvin) Pipe of ASTM 312 TP 304 L is suitable?

Dear Vivek,

Please let me share the following info I have on this subject: 


Cryogenic Steel ASTM A553 Type 1 and  Type 2, / ASME SA-553/SA-553M Q&T 8% and 9% Ni-alloy Steel.  

Ideal for containment or transportation of liquefied gases such as LNG, oxygen, nitrogen and argon which need to be stored at a temperatures below -196°C. The material is good for any pressure containing application with excellent resistance to low temperature brittle fracture.
Many of the pressurized storage tanks designed to hold these gases are double walled with an insulation layer to minimise any generation in heat. Considerations should be made not only to the material used but also the fittings required which will also include piping and valves.
Other Cryogenic Steel Grades
You may also consider the following steel grades for cryogenic purposes:
 
Best Regards,
Shashank C Vagal  (Quality Adviser)
Neo Metal-Analyst & NDT Services (Approved by IBR, Thermax, AERB)
Regd Office: 301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA
Tel: +91 22 2611 6640 / (+91) 9821386292 /  8082395502 / 9819191861    
Works Office: A-25, Geet Siddhee, Sector No. 11, Pradhikaran, Gat No. 62, Boradewasti, Moshi, Dist: Haveli, PCMC, Pune – 411044, Maharashtra, India   
www.neometalanalystndt.com / enquiry@neometalanalystndt.com / nach_sam@yahoo.com




From: vivek singh Chaudhary <viveksinghme1612@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, 5 December 2016 11:02 PM
Subject: [MW:25795] For Cryogenic Services at Temp -196 degree Celsius (17 Kelvin) Pipe of ASTM 312 TP 304 L is suitable?

Dear Experts,
Currently I am working on a project of ISRO (Indian Space Research Organisation) for Integrated Cryogenic Engine Testing Facility (ICET), for bidding in that services are Liquid Hydrogen, Liquid Oxygen, Liquid Helium, Liquid Nitrogen, Gaseous Hydrogen, Gaseous Oxygen, Gaseous Nitrogen, Gaseous Helium.
For SS Seamless Pipes client has given three options for material ASTM 312 TP 304L/ ASTM 312TP 316L/ ASTM 312TP 321. 
Kindly suggest me the suitable material for the same that gives economical and best design.

Thanks in advance.

Regards:-
Vivek Singh Chaudhary
Piping Design Engineer.
Contact No.- +91 9990441755.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP6FfyH8HRZ%3Dk7QQbBvHyjqSCXryhuoGtrw%2BHJ4_aKcSrp0fHg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/kkfywtcumtgl865xgiwb3op0.1481564935234%40email.android.com.
For more options, visit https://groups.google.com/d/optout.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...