Re: [MW:25813] Temporary piping used in hydrotest - ASME B31.1

Thank you for sending.

Could you please inform for the reference for the table from code, standard.

Kind Regards.



2016-12-10 7:58 GMT+01:00 'Shashank Vagal' via Materials & Welding <materials-welding@googlegroups.com>:
Hello Zakaria,
Please see below
 
Best Regards,
Shashank C Vagal  (Quality Adviser)
Neo Metal-Analyst & NDT Services (Approved by IBR, Thermax, AERB)
Regd Office: 301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA
Tel: +91 22 2611 6640 / (+91) 9821386292 /  8082395502 / 9819191861    
Works Office: A-25, Geet Siddhee, Sector No. 11, Pradhikaran, Gat No. 62, Boradewasti, Moshi, Dist: Haveli, PCMC, Pune – 411044, Maharashtra, India   
www.neometalanalystndt.com / enquiry@neometalanalystndt.com / nach_sam@yahoo.com



From: Zakaria ghrab <zakaria.ghrab@gmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Saturday, 10 December 2016 8:10 AM
Subject: [MW:25809] Temporary piping used in hydrotest - ASME B31.1

Dear Experts,

  Could you advise us: For piping system hydrotests power plant project, we ave to prepare and use some temporary piping. The issue is :

- Is it Manadatory to perform NDE in related welds  and also PWhT
NO FOR EITHER, 
BUT FOR PWHT - ANY WELDING INDUCED STRESSES IN EXCESS OF YS MAY BE UNDESIRABLE.
PERFORMING NDE ON ALL INCLUDING TEMPORARY MEMBERS WILL BE IN YOUR BEST INTEREST. IF A JOINT LEAKS BECAUSE OF ANY WELD DEFECTS, YOU WILL FACE EXTRA COST, ADDED TIME, RE-SCHEDULING, ETC  DUE TO  RE-HYDRO.
- For Flange fabrication, how to use plate thickness, any code or standard reference !
PLEASE SEE ATTACHED


Please advise according your experience and with ASME reference .

Thank you.

--

Thanks and Regards, ?
-----
زكرياء غراب
GHRAB Zakaria 
Tunisia : +216 96 635 805

Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD8EeB15hqZTM7eP9EyGTUCdawvDKKHZxHHC%2BK5NhRbeOLt8YQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1461469163.207663.1481353081256%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.



--

Thanks and Regards, ?
-----
زكرياء غراب
GHRAB Zakaria 
Tunisia : +216 96 635 805


Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD8EeB0tGZC%2BpOOwgiEAttxTSe_gVzed0C469z1GjBqvDPRr5g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...