Hi Pradip 
My suggestion is AWS D.10.10/D10.10M: 1999(R2009) – Recommended. Practices for Local Heating of Welds in Piping and. Tubing.
Kind regards 
Sent from my iPhone

On 1/07/2016, at 4:56 pm, pradip kumar Sil <pradipsil@gmail.com> wrote:

Dear Everybody,
How many thermocouple to be  attached in the weldment during Pwht  / During Preheating , we are following as per  Project Specification.

My Question is anywhere in the code/ Standard  is it mentioned ? Pls refer
Thanks in advance
Regards
Pradip  

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8kLFfRTB_R82axYxBN8dEJPvfpJhY%3Ddm2seXUp7wd3B4Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...