Dear Pradip,
As per API minimum 2 thermocouple shall be used and it' will be increased based on the diameter of the weldment.
Thanks & regards,
M.Sudalai.
On 1 July 2016 at 07:56, pradip kumar Sil <pradipsil@gmail.com> wrote:
Dear Everybody,--How many thermocouple to be attached in the weldment during Pwht / During Preheating , we are following as per Project Specification.My Question is anywhere in the code/ Standard is it mentioned ? Pls referThanks in advanceRegardsPradip
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8kLFfRTB_R82axYxBN8dEJPvfpJhY%3Ddm2seXUp7wd3B4Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BZM_eY71yPm4o8NwVK7Cv2x3SoovoR5czojO18yvAG8uutYNQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments