Re: [MW:25145] PWHT Requirement as per ASME B31.3 Ed.2014

Lot of changes taken in Power and Process piping. 38mm requirement of P1 for sec8 and sec1 not for piping?

On 25-Jul-2016 7:05 pm, <dilintas@gmail.com> wrote:
All codes require PWHT for carbon and low alloy steel if thickness greater than 38 mm

Sent from my BlackBerry 10 smartphone.
From: 'wilfred kojo' via Materials & Welding
Sent: Σάββατο, 23 Ιουλίου 2016 - 19:34
Subject: Re: [MW:25140] PWHT Requirement as per ASME B31.3 Ed.2014

Loni,
The 38mm stated is based on code requirement or personal judgement. Please if by code requirement, state the code and section of the code referenced.
 
Krishna,
You are only mandated to perform PWHT if it was initially stated in WPS or design requirement. Outside these, based on code requirement, it is not mandatory.
 
Regards,
 
Wilfred Kojo
AWS CWEng


On Saturday, 23 July 2016, 14:36, 'wilfred kojo' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Krishna,
Base on requirement of the spec. it not required as long as both conditions for exemption are met.
 
Regards,
Wilfred Kojo
AWS CWEng


On Saturday, 23 July 2016, 7:49, Krishna Mudhale <kmudhale@gmail.com> wrote:


Hi Experts,
I would like to know about PWHT Requirement as per ASME B31.3 Edition 2014.
Actually for P1 Material as per Table 331.1.1 given Soaking Temperature & time for all thicknesses.
Also as per Table 331.1.3 given some exemption for PWHT of P1 material subject to two limitations ie. One for greater than 25mm thickness a preheat of 95 Deg C to be applied whereas other one is for greater than 5mm Thk multiple layer of Welding carried out.
So my question is, If thickness is of 50mm and if we are covering both the condition of preheat and multiple layer Welding then PWHT is applicable or not?
Kindly need your advise...
Thanks & Regards
Krishna Mudhale
Mob.:+91-9860459776
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG8LsMacsw5LMv27PSeN_DzEHztwhkpdHpn2qxOREF3SX_0MXw%40mail.gmail.com?utm_medium=email&utm_source=footer.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1259855024.6068870.1469261200741.JavaMail.yahoo%40mail.yahoo.com.

For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1002386492.6216925.1469282441464.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160724181750.6713429.82985.3831%40gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN0TYJ%2By2rps7LwWGdQQ-bDJxgx%2BE4V-p-Le-oEqcCB6g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...