Saturday, July 2, 2016

[MW:25047] Re: Thermocouple Quantity

You may get some detail in WRC Bulletin 452.

Normally for for ASME vessels, number & location of Thermocouple shall be in compliance with temperature variation during heating, cooling and holding time with respect to specified span of length.

Regds/Jignesh 

On Friday, 1 July 2016 14:02:22 UTC+5:30, pradipsil wrote:
Dear Everybody,
How many thermocouple to be  attached in the weldment during Pwht  / During Preheating , we are following as per  Project Specification.

My Question is anywhere in the code/ Standard  is it mentioned ? Pls refer
Thanks in advance
Regards
Pradip  

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ec36c920-ff8b-4a76-9e7c-9115425c42de%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...