use NiCr3 and do Stress relieving
THANKS & BEST REGARDS,
KG.PANDITHAN, IWE, AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
On Mon, May 9, 2016 at 7:54 AM, Ravi <meshekhar@gmail.com> wrote:
you can use E/ER 308 electrode for filler material.--See more details here: Welding AISI 430 to AISI 1020Ravi
On Wednesday, April 27, 2016 at 6:40:28 AM UTC-5, mhaskar aly wrote:Dear Friends,KIndly suggest filler metal for joining AISI 430 with S355J2HThanks & Best regardsAly
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/48c36942-fe17-4d4e-85e2-d06cfa14474f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOto8vL%3DLJ9UMbOQyPOo%2ByUwte9zCr6sWUixr%2BzdHKrxg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment