Re: [MW:24774] Re: PERFORMANCE QUALIFICATION

if it is part of B31.1, u need not qualify because it comes under non pressure part for which ASME sec 9 qualification is enough provided all essential variable meet. 

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Sun, May 8, 2016 at 8:32 AM, Chip Frizzell <chipfrizzell@gmail.com> wrote:
Pipe supports do not necessarily fall under structural. If welding pipe supports not required to be qualified to D1.1 by specification, then qualification to 31.1 will cover the welding of the support.  



Chip Frizzell


Sent from my iPhone

On May 7, 2016, at 1:55 AM, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:

Acceptance of ASME WPS in D1.1 is purely owners engineer decision, If rep of client want new WP  as per D1.1, yes u have to do

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Sat, May 7, 2016 at 9:31 AM, <thai-dv@alpha-ecc.com> wrote:
Dear sir,
first, please check project specification mention or not.
second,
ASME IX (QW- 300.2): "  These paragraphs require that each manufacturer or contractor (an assembler or an installer is to be included within this premise) shall be responsible for conducting tests to qualify the performance of welders and welding operators in accordance with qualified Welding Procedure Specifications". It's mean when you carry out WQT, you shall follow WPS. So that, if your WPS can use for both ASME B31.1 and AWS D1.1, you no need to qualify welder again. BUT almost project specification require separate WPS for ASME  IX and AWS D1.1. 

Vào 09:48:13 UTC+7 Thứ Bảy, ngày 07 tháng 5 năm 2016, Mac Palola đã viết:


Dear Sir,

(B31.1 Code) We have a qualified pipe welder with 6G position (18.26 thickness test coupon), as per ASME Sec IX Table QW-461.9, he is qualified for all positions for groove and fillet weld - plate and pipe.
This qualified welder was task to weld pipe support (H Beam), It has been questioned by the TPI that this welder should be qualified again as per AWS D1.1.
My Questions are;
1. Should we qualify this welder again as per AWS D1.1? If yes, what is the supporting code for this.
2. Does ASME Sec IX Rules for this situation?

Need your advise.....


Thank you

Mac Palola



--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a8c2dddd-d6dd-4b9f-9f45-3f4f410ab5c5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOmQzNN7X%3Dd3-d5boyutgRM0n375q%2Bkm9bBa_%3D7Obg7vw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CCC409FF-D995-406C-BAC4-304C94A455B3%40gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMa6jOe0PPtxyH_QNbVpyY3W9_gMcrgi4cKnPJ0uvwHOg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...