Re: [MW:24916] Combination of PQRs

As you stated , to combine 2 PQRs and generate a new WPS, your PQRs should be performed with material greater than 13mm.

2016-05-31 11:14 GMT+03:00 Demir Alp ILIKOBA <demiralp85@gmail.com>:

Dear Experts; 


  I would like to get your professional opinion on combination of PQRs as per ASME Section IX QW-200.4   I have 2 PQRs (w/back-gouging) and I would like to combine these 2 PQRs ;

·         PQR-1 Base Metal P355 GH Thickness : 8mm Process 1)Root : SMAW 2)Hot-Fill-Cap : SAW Back Weld: SAW 

·         PQR-2 Base Metal P355 GH Thickness : 8mm Process 1)Root : SMAW 2)Hot-Fill-Cap : SMAW Back Weld: SMAW  

 

My question is whether i can combine these 2 PQR for generating a new WPS ;                

·         Generated WPS : Base Metal Thickness : 16mm Process 1)Root : SMAW 2)Hot-Fill-Cap : SAW Back Weld: SMAW

 

Is it possible to use PQR-1 & PQR-2 for generating WPS for usage of SMAW for the back weld ?  What bothers me and makes me feel i should get advisory is since QW-200.4 (b) says;  For GTAW, SMAW, GMAW, PAW, and SAW, or combinations of these processes, a PQR for a process recording a test coupon that was at least 1/2 in. (13 mm) thick may be combined with one or more other PQRs recording another welding process and any greater base metal thickness.  Since my PQRs are carried out with 8mm thck. is it possible for me to combine them and apply SMAW Back Weld instead of SAW or not? 

Best Regards;

Demir

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACj12PCk4tK3uVEu5h4%2BAbqpA6Z7s8pSw0s7XfnjXv9FLOnG1Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--

Saygılarımla / Regards


Tuğrulhan ÖZDEMİR

API 653 AI, Welding & Materials Eng.

ASNT VT, PT, MT, RT L-II

+90 539 747 2676


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABSWRjoWNC5xA4j9tqPCrUkrgZD98xe6jOa%2BDVDr9K8agFFKiw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...