Friday, May 6, 2016

[MW:24761] PERFORMANCE QUALIFICATION



Dear Sir,

(B31.1 Code) We have a qualified pipe welder with 6G position (18.26 thickness test coupon), as per ASME Sec IX Table QW-461.9, he is qualified for all positions for groove and fillet weld - plate and pipe.
This qualified welder was task to weld pipe support (H Beam), It has been questioned by the TPI that this welder should be qualified again as per AWS D1.1.
My Questions are;
1. Should we qualify this welder again as per AWS D1.1? If yes, what is the supporting code for this.
2. Does ASME Sec IX Rules for this situation?

Need your advise.....


Thank you

Mac Palola



--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b80e7fe7-f740-4f4f-af13-4543f42b31a2%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone