Dear,

If i have to replace RT with UT as per API 650 then appnedix U will be applicable.

Can anyone tell me what will be the best combination for Vertical and longitudinal joints and for intersection of vertical and horizontal joints?

Shall i go with TOFD and PAUT for upper and bottom zone which will be not covered under TOFD.

tanks thickness for plate to plate 10mm#10mm and 10mm#12mm till 32mm#32mm and 32mm335mm.  

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3998b3a6-9773-4450-912f-563fc2ef1346%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...