Re: [MW:23601] Hardness without pwht

Hai,
Normal carbon steel after PWHT accepted in 31.3 P1 to P5 but alloy maternal not accepted in same standard.
Regards,
PETER SOLOMAN
Sr.QA/QC Enr

On Tue, Sep 29, 2015 at 12:57 PM, elias jarjoura <elias-jarjoura@hotmail.com> wrote:
Dear Sombir ;

Most ITP (inspection test pack ) amends Hardness testing after PWHT .
Keep in mind that witnessed hardness test will require presence of RT report and PWHT report and thermal graph.
purpose of hardness testing is to verify that stress relief was properly done and base metal  is in the right eutectic phase .

Regards 
Elias 

> Date: Tue, 29 Sep 2015 01:03:56 -0700
> From: sombir.jangra009@gmail.com
> To: materials-welding@googlegroups.com
> Subject: [MW:23590] Hardness without pwht

>
> Dear sir,
> We can do hardness prior to pwht. Please go ahead and do it without any hesitation and cross check it with given table.
> Also in some cases we can exempt pwht if hardness value finds within range. For this please refer ASME code.
> Thanks and regards,
> Sombir
>
> --
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> Visit this group at http://groups.google.com/group/materials-welding.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5e34cac1-3775-4147-bb43-5de7165d87b3%40googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/DUB113-W131AE6C3FCF1184BDAA7C6B8A4E0%40phx.gbl.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMvP5szpeUAeHwR1JS%3DzisWW0vGadeWWodkJUD4DEO2ER0fOfQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...