Dear Sir,
I have taken lots of trial for SAW welding.
I got good result with the parameters but its not consistent.

Material - SA240TYP304
Filler- ER308L
Parameter- 340 to 390 Amp, 32 to 34 Volt, 300 to 325 mm/ min.

I have maintained interpass - 150 C as well as all the requirements needed for the welding.

Pl guide me for getting good impact (27 joules / 0.38 mm lateral expansion) property at -196C.

Regards,
Chandan sharma

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTWUJJksnR4r6NkwTzkYK1RV6xDXbc4rjFjN%2BfH4H_Bc_T3fg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...