[MW:23569] Re: Is it possible to qualify two welders on same test coupon

it depends. According to qw-360 any welder should weld the thickness welded in WQT. for example if you have the thickness of 120 mm and the wqt said that the welder should weld 20mm thickness you can use this welder for welding 20 mm once.

On Tuesday, September 22, 2015 at 5:56:35 PM UTC+3:30, waqas suleman wrote:


On Tue, Sep 22, 2015 at 5:05 PM, waqas suleman <waqas....@gmail.com> wrote:
Dear All,

Can we use two welders for qualification of WQT using by combination welding (GTAW+SMAW) on single test coupon.
I used 16" pipe sch-30 for WQT. As per  ASME Sec IX, QW-306 my interpretation says it is possible.
Looking expert judgement from respected group members.


Regards,


Waqas Suleman
Construction Manager
Mobile # 00966 59 359 0798

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/77db634f-e823-43dc-9fe3-503819fb0c1f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...