I think it depends to design engineer


On Sunday, September 13, 2015 at 1:44:10 PM UTC+3:30, ALAM wrote:

Can we accept hardness without pwht.(talking about weld portion only)I.e joints .
Second question is in any metal pipe manufacturing system ,they are checking the hardness test without pwht of a pipe or joints.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7fc597cb-d2f7-40fa-87a3-d4a41344ff78%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...