Friday, September 25, 2015

[MW:23537] Forging material Cleanliness

Dear experts 


Forgings Shall meet a material cleanliness C2/R2/S2 rating , as described in  ASTM E381.


Kindly clarify the above statement . i couldn't find anything in ASTM E381......

Thanks in advance

Selastine 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/26d289fd-e0d8-4685-8a0c-fe66b3df999a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...