Wednesday, July 29, 2015

Re: [MW:23229] reg: Test coupon thickness range

Prince,

Input your variables here and know the range:

http://www.gowelding.com/wp/calc3.htm

ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,

Nandesh Kumar Arasappa

P.S. : Please don't print this e-mail unless you really need to.

--------------------------------------------
On Tue, 28/7/15, Prince C thomas <princecthomas@gmail.com> wrote:

Subject: [MW:23220] reg: Test coupon thickness range
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Tuesday, 28 July, 2015, 12:13 AM

Dear all,
 In our district cooling CS ( ASTM A106 Gr,B)
pipeline project, pipe wall thickness is from 3.2 mm to
20.62 mm.  and our WPS is qualified and now we have to
conduct welder qualification test.So what is the minimum  
test coupon  thickness we should select so that welder can
weld upto 20.62 mm thickness pipe during
production.
WPS Details:
Welding process: GTAW & SMAW
Base metal thickness range : 5 - 22
mm
Weld metal groove for GTAW ; 6mm and SMAW - 16
mm


Prince C Thomas



--

You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.

To post to this group, send email to materials-welding@googlegroups.com.

Visit this group at http://groups.google.com/group/materials-welding.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0fdce533-3131-4418-bec0-6f0cef76fb24%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1438110511.10277.YahooMailBasic%40web193601.mail.sg3.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...