Monday, July 6, 2015

[MW:23139] RE: 23138] Welding of Had field steel

Hi Hrushikesh.
 
Hadfield or Austenitic Manganese steels are very specific to few good foundries.Welding of this grade of steel (mostly casting) requires specific skill, welding electrode selection and control of welding parameters. Here're some general guidelines on welding of this alloy. What grade Hadfield steel is being welded? what's the section thickness involved. These  are some of the key variables in  successful welding of this grade of steel.
 
You may contact these manufacturers for welding consumables and further info.
 
Thanks.
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineer/Specialist
Ontario, Canada
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Hrushikesh Sangamnerkar
Sent: Sunday, July 05, 2015 9:17 AM
To: materials-welding@googlegroups.com
Subject: [MW:23138] Welding of Had field steel

Hi..
Anyone has experience of welding Hadfield steel?

Hrushikesh H Sangamnerkar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2q1NBcWCZkdO1jxbHMjpcWCPvcnP4%2BKuizfX3HAgDkqkw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...