If I remember correctly, L&T Hazira did titanium matl heat exchanger, wall thickness 9 or 12 mm in 1995 in light fabrication shop with TIG process.
Regards,
S.SENTHILKUMAR
S.SENTHILKUMAR
On Monday, 27 July 2015 2:13 PM, Hrushikesh Sangamnerkar <hrushi612@gmail.com> wrote:
Sir,
Thank you for this information. As far as GTAW is concerned we have much of expertise.
Thank you for this information. As far as GTAW is concerned we have much of expertise.
We had also enquired at DRDL,HAL etc. But they regreted.
For BARC, haven't enquired as I didnt get any contact. If u have any pl share.
If that also doesn't work, what u suggest? I think SAW to be carried.
Thank you.
Hrushikesh H Sangamnerkar
On Jul 27, 2015 10:50 AM, "Muthukrishnan Sivaramakrishnan" <smkro3@gmail.com> wrote:
Dear Mr.Sangamnerkar,I doubt about the capabilities of EBWs available in India to meet your demand .For 3 to 4 meter diameter you have to use partial vacuum EBW system which works in open air .Such a facility was demonstrated by SCIAKY ,Frnace in 1776 if I remember correctly during my training at this facility and I participated in this programme. We welded 80 mm thich SS 316 vessel of dia same as yours .In this system the EBW gun will move along the vessel covering the joint area with a special partial vacuum system . OSAKA university people developed another machine in which the vessel is kept in a vacuum room and the beam is impinged on the vessel mounted on a rotary positioner .For your immediate use please use normal TIG welding and a roller positioner rotate the vessel. Please inform your location ,vessel dimensions and code requirement .If you need an welding expert to visit you for procedure qualification with TIG please inform .Regards,S.Muthukrishnan--On Sun, Jul 26, 2015 at 12:09 PM, Hrushikesh Sangamnerkar <hrushi612@gmail.com> wrote:I have shell Dia. Of 3-4 meters. Are they doing EBW with the above mentioned diameter also?Hrushikesh H SangamnerkarOn Jul 25, 2015 8:06 AM, "Hrushikesh Sangamnerkar" <hrushi612@gmail.com> wrote:--Gm all,
Anyone experienced in EBW of titanium?
Pl share. Suggest any vendor who has this facility, if any.Hrushikesh H Sangamnerkar
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2o_6y2__XcWzAhXo6f_JvTOLCJZFxeH%3D-V%3DiyUK%2BWggbA%40mail.gmail.com.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAB-sOHSUmmw08O4P4J-nF205PohdFHpJECmT134aMC-7oXzQw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2rzpXVXGSVFZasFdRMMoYMseXUd9SbKpFZNzhiN4NtUoQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments