Re: [MW:23142] Re: PWHT on Channel or bonnet of HX with 6 or more tube passes

Any precaution need to be taken during pwht, especially to avoid any distortion? We have faced a problem before that after pwht, the bonnet was leak at the flange joint after installed and need to be clamped, tq in advance sir

On Jul 6, 2015 4:16 PM, "Hemant Solanki" <shm8324@gmail.com> wrote:
in 6 or more passes there will be more welding on surfaces within close proximity. Such welding will make parent metal hard and brittle... in order to avoid such problem, PWHT requirement is added by API, so that parent metal becomes soft and adhere to its properties.


On Sunday, July 5, 2015 at 8:18:46 PM UTC+5:30, mrshiha wrote:

Can anybody explain to me why its stated in latest API660 for this requirement? Its not stated any reason why is shall be PWHT due to lethal sevice or regarding thickness

Shiha

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/121d03d5-1651-4eb2-b5c3-a7c8797c9703%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BidF71HfPm%3DrTrcBKyC6x6w%3DyGVu%2B7iVojOVGc15JuoDA-Ccw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...