Re: [MW:23203] Hydrotest after Addl. Nozzle provision

only non-structural small attachments may be welded to the tank in accordance with 7.2.1.12 after hydro static test


On 26 July 2015 at 10:21, Thota Kishore <krish.royal18@gmail.com> wrote:
Dear Members,

We have constructed API 650 storage tank (28m Dia x 16.5m HT), hydro test, painting and calibration has been completed. But now client requires additional 10" nozzle in the tank. 
If i provide 10" nozzle now, whether i have to do hydro test again or pneumatic test is sufficient. If so, please let me know the clause with Ref. Std.
Kindly suggest me.

Thanks in Advance.
Regards,
Kishore Thota

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVub%3DRn%3DjGwVuDzKjQxz%3DBeqpP2nQ7JhTinUbHze-fu7AzQg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...