Dear Prince,
It should be either 10.31mm or any thickness with 3 layer.

Regards
Biplab Pal

On Mon, Jul 27, 2015 at 11:13 PM, Prince C thomas <princecthomas@gmail.com> wrote:
Dear all,

 In our district cooling CS ( ASTM A106 Gr,B) pipeline project, pipe wall thickness is from 3.2 mm to 20.62 mm.  and our WPS is qualified and now we have to conduct welder qualification test.So what is the minimum   test coupon  thickness we should select so that welder can weld upto 20.62 mm thickness pipe during production.

WPS Details:

Welding process: GTAW & SMAW

Base metal thickness range : 5 - 22 mm

Weld metal groove for GTAW ; 6mm and SMAW - 16 mm



Prince C Thomas

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0fdce533-3131-4418-bec0-6f0cef76fb24%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFnzQg3YW70otj61R1_OqN%3DbR5L1Ki5Lsk4sEz3%2B8pztquSMyw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...