Sunday, July 26, 2015

Re: [MW:23201] EBW in titanium for T>50mm

WRI EBW machine was installed by me about 35 years back .It is not in operation now .

muthukrishnan

On Sat, Jul 25, 2015 at 11:25 AM, 'SENTHILKUMAR SWAMINATHAN' via Materials & Welding <materials-welding@googlegroups.com> wrote:
In addition to above locations, WRI - BHEL Trichy has EBW.  
Regards,
S.SENTHILKUMAR



On Saturday, 25 July 2015 7:50 AM, Muthukrishnan Sivaramakrishnan <smkro3@gmail.com> wrote:


Dear Mr.Hrushikesh,

 BARC ,Bombay , DRDL ,Hydrabad and GTRI ,Bangalore have EBW facility .Please contact them .

Regards,
S.Muthukrishnan

On Sat, Jul 25, 2015 at 5:36 AM, Hrushikesh Sangamnerkar <hrushi612@gmail.com> wrote:
Gm all,
Anyone experienced in EBW of titanium?
Pl share. Suggest any vendor who has this facility, if any.
Hrushikesh H Sangamnerkar
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2qQB-GG%2BMqqSvZsP1u%2Ba1y1wT-6Ha-QXvs1JT8fHcdpzQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAB-sOFnutpmHTSJzwq3N-qcmmFoYGYAqEaws6VAJx5ntZu3%2Bw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1286838211.1463778.1437812742303.JavaMail.yahoo%40mail.yahoo.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAB-sOEsv%3DRtHbwgEtbGjUWFijpRKUUr%3DJT%3DTyBdqv1xmnardA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...