[MW:23148] Want to understand the "Product analysis"

Dear Mentors,
For Material ASTM A516 Gr 70 the client requirement is based on product analysis. Does that mean that all plates shall be tested for product analysis? or certain plates from that heat is enough to report that as product analysis.
Thanks in advance for your kind advise if possible with citation.
Best regards,
Umar.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fcb537c5-a82e-48e0-be72-29ab2456398a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...