[MW:23206] Re: EBW in titanium for T>50mm

I have shell Dia. Of 3-4 meters. Are they doing EBW with the above mentioned diameter also?

Hrushikesh H Sangamnerkar

On Jul 25, 2015 8:06 AM, "Hrushikesh Sangamnerkar" <hrushi612@gmail.com> wrote:

Gm all,
Anyone experienced in EBW of titanium?
Pl share. Suggest any vendor who has this facility, if any.

Hrushikesh H Sangamnerkar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2o_6y2__XcWzAhXo6f_JvTOLCJZFxeH%3D-V%3DiyUK%2BWggbA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...