Sunday, July 26, 2015

[MW:23206] Rivetted like object in piping

Dear Experts
 
Is any body experienced with indication on piping with attached pictures. I observed it in 48 " carbon steel piping.
 
please advice
Thanks & Regards

PRADEEPKUMAR HORMIS


 
 


 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE2abXm7cepY_WAxvRNrcSYp6%2BQHsMBss4j3dsSBP%2B6jZNdbxg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint