Good day Mr Thomas. Dr George is correct. Please note however that your WPS does not cover you to weld  3.22mm up 4.99mm.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of george.dilintas@gr.bureauveritas.com
Sent: 28 July 2015 11:48 AM
To: Prince C thomas
Subject: Re: [MW:23224] reg: Test coupon thickness range

 

Your thickness divided by 2

 

Sent from my BlackBerry 10 smartphone.

From: Prince C thomas

Sent: Τρίτη, 28 Ιουλίου 2015 - 06:10

To: Materials & Welding

Subject: [MW:23220] reg: Test coupon thickness range

 

Dear all,

 

 In our district cooling CS ( ASTM A106 Gr,B) pipeline project, pipe wall thickness is from 3.2 mm to 20.62 mm.  and our WPS is qualified and now we have to conduct welder qualification test.So what is the minimum   test coupon  thickness we should select so that welder can weld upto 20.62 mm thickness pipe during production.

 

WPS Details:

 

Welding process: GTAW & SMAW

 

Base metal thickness range : 5 - 22 mm

 

Weld metal groove for GTAW ; 6mm and SMAW - 16 mm

 

 

 

Prince C Thomas

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0fdce533-3131-4418-bec0-6f0cef76fb24%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20150728094742.6459475.73449.11865%40gr.bureauveritas.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...