Wednesday, July 15, 2015

[MW:23165] Economizer tube crack

Dear All, please support to investigate the crack of ecanomozer tube.as attached picture

    Type of tube- spirlly finned tube
     spiral material-sa-178a
     tube dia meter-219.1mm
      tube material-106b
       Maximum design pressure-5800kpa
     

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c13d642e-800f-4c71-a00e-72f809b0eac6%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...