Dear P C T,

You can select 6"  SCH 80/XS  (t=10.97 mm)
or
8"  SCH 80/XS  (t=12.7 mm) pipe test coupons for this purpose.

JijiLal K.M.,Welding Engineer,
Al banna Engineering LLC.
BPCL Kochi refinery expansion project.

Jiji Lal K M
# 9846128141

On 28 July 2015 at 01:43, Prince C thomas <princecthomas@gmail.com> wrote:
Dear all,

 In our district cooling CS ( ASTM A106 Gr,B) pipeline project, pipe wall thickness is from 3.2 mm to 20.62 mm.  and our WPS is qualified and now we have to conduct welder qualification test.So what is the minimum   test coupon  thickness we should select so that welder can weld upto 20.62 mm thickness pipe during production.

WPS Details:

Welding process: GTAW & SMAW

Base metal thickness range : 5 - 22 mm

Weld metal groove for GTAW ; 6mm and SMAW - 16 mm



Prince C Thomas

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0fdce533-3131-4418-bec0-6f0cef76fb24%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHjakWdUPOn4p__5SMFTNu2_XkkTF%2BCEWTh%2BuLuQ%2BMrnQQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...