[MW:23214] Re: Welding of Had field steel

Sir,
Thank you for the input.

Till now we carried out welder quickly quali. We are facing problem in PT. Though we are hv smoothly grounded the crater points at start stop locations.

Hrushikesh H Sangamnerkar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2rRfLmL%3Dfcx_sHuvqEEmgpkEiBmtgL4GL5DB%2BM%3DbBjQsA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...