Misalignment / Mismatch causes

1. Point of stress concentration due to uneven load from the fluid
2. Point of erosion & wear due to fluid
3. Point of corrosion due to fluid.
4. Area of reduced strength
5. Causes the fluid turbulent

 
Thanks & Regards
J.Gerald Jayakumar
0091-9344954677


From: Sandeep Maan <sandeepmaan6861@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Wednesday, July 22, 2015 3:30 PM
Subject: [MW:23182] Defects Due to misalingment during Fit-up

Dear Experts

 Kindly let me know the what will be the possible Effects arise due to mismatch/misalignment During fit-up
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a13fe7c2-d861-4f6b-a9d3-ce40b8a43f40%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...