Re: [MW:23169] PQT FOR A333 Gr.6 Material with PWHT

ER 807NI1 FOR ROOT AND HOT PASSES
FOR OTHER PASSES U CAN USED E7018 H4R


Regards,

Joydev Dalai
   

On 15 Jul 2015 10:22, "Siva Chidambaram" <mechsivachidambaram@gmail.com> wrote:
Hi,
 
I need to prepare WPS & PQT for the A333 Gr. 6 Material with PWHT as per ASME B31.3 with GTAW + SMAW process  & GTAW + FCAW.
Can anybody suggested what electrode shall I use for the process.
 
Thanks
M. Sivachidamabaram 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPJQpMV4LCnpAL%2BEaywhFg6MiDpXkHATSKu_vF9z9xpOJgDefA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFQz-VL91RATQzb7FSOta0djXN6aqQ2CQufx-ntGn6zWQRiLYg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...