Re: [MW:23199] We are facing minor pore defects in CuNi 90/10

you can use the camera technique, filling your tube with argon, argon more protection with your filler, ie, argon inside and out.

2015-07-25 6:14 GMT-05:00 Vanchinath S.A. <vanchinaths@gmail.com>:

You may try argon+1.5%Hydrogen as shielding gas.

On 25 Jul 2015 10:15, "Nazz A" <nazzimmm@gmail.com> wrote:
Sir  I am Muhammad.

we are working here in qatar under Qatar Petroleum.  We have to  complete the fire line systrm through Cu Ni.  We are using Tig welding and ising monel 67 CuNi filler wire. With goving back purging as Argon 99.99 % composition.

But still we arr facing the defects as porocity.  We already covered the area and clean the parent metals and filler wire. Using all of materials like cutting disk wire brush clits and everything is non ferrous.  Our present climate is summer here in Arabian dessert.

But in the Radiography,we cant controle the porocity here. Our all welders are wrll expetienced and well occupied. The poricity is always minor and when we cut out and checking its cant show.

Our acceptable criteria is lower than 0.6 mm.

I hope that you will give the right solution on our problem.

Yours regards...

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/193c15ab-9484-4301-a2dc-abbc4438e166%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B6Tn1%2B5A_O7fm%3D5tg9Vs3CEGxhu2NFoUat7e7awTwKV2pzE0A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--

Ing. Jose Juan Jimenez Alejandro

Cel. 8116171750

Skype: jjjimeneza

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5Zur%2BiogOA6-mVn%2BA_wxkS66p_mbwg5qRZMiHs_M5PxGAaOQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...