Thursday, July 30, 2015

[MW:23230] Hardox to Hardox Butt welding joints

Dear Experts,

We need to do butt welding of Hardox 400 Plates thk 20mm for one of our projects. Could any body suggest me which electrode  to be used.

Best Regards

Vheerrajhu

--