Re: [MW:23197] Welding of Pressure Vessel Parts

Not allowed to transfer GMAW short, clearly specified that the prequalified WPS D1.1 and ASME IX also has some limitations thereon, it can be used this process but in spray transfer GMAW, check it well in the codes.

2015-07-25 6:24 GMT-05:00 Vivek <vivek.anuj.jain@gmail.com>:
Dear Experts
My question is that is ASME Sec VIII or AWS D1.1 or any other codes Prohibit manufacturer to use the GMAW welding process, and if we can use GMAW welding what care we should take while welding Parts of Pressure Vessels
In general i have seen people using TIG welding or SMAW welding , sometimes FCAW too but why not GMAW

Thanks
Vivek

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9d79b199-9c5e-43c4-ae08-28fd106a8328%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--

Ing. Jose Juan Jimenez Alejandro

Cel. 8116171750

Skype: jjjimeneza

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurLnFCF%2B3tcRsUMZ4QLZS7nTkKdEGNAZdt31KTJoBm0jVw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...