no, because dia of qualification is >73mm, but ur job calls for 50mm. ( I think u have qualified welders in Plate)
THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY
On Thu, Jul 3, 2014 at 5:37 PM, <george.dilintas@gr.bureauveritas.com> wrote:
Is the F no of the wires the same as in the qualifications?
If yes, he can.
Take care also of the other essential variables like current and polarity, innert backing for GTAW, short circuit thickness limitation, inner backing and transfer mode for FCAW
best regards
Dr. Georgios DilintasI&F REGIONAL TECHNICAL MANAGER
Authorized Nuclear Inspector
Authorized Inspector Supervisor
BUREAU VERITAS HELLAS
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
(See attached file: Dilintas_George.vcf)"rajesh s. mhaske ,Engineer Welding ,PUNE,INDIA" ---27/06/2014 11:58:10---Dear sir Pipe dia : 323.*33 mm thk
From: "rajesh s. mhaske ,Engineer Welding ,PUNE,INDIA" <rajesh.mhaske17@gmail.com>
To: materials-welding@googlegroups.com
Date: 27/06/2014 11:58
Subject: [MW:21285] QW-452.3 GROOVE-WELD DIAMETER LIMITS
Sent by: materials-welding@googlegroups.com
Dear sir
Pipe dia : 323.*33 mm thk
Tube dia : 50.8 *6.35 mm thk
Groove design for above pipe to tube welding : set in (groove on header ) / set on (groove on tube )
Welding process : GTAW + FCAW
Qualification of welder: OD >73 mm and Thk - Max to be welded with process GTAW+FCAW
Question :
1) Can above qualified welder be deployed for welding of set in and set on joint.
--
To post to this group, send email to materials-welding@googlegroups.comhttp://materials-welding.blogspot.com/
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment