Hi,
As per ASME Sec.VIII Div.1, PTC is required only when the subject
material is not exempted from impact requirement. Refer clause
UG-84(i) for more clarification about PTC requirement.
On 7/3/14, PURUSHOTHAMAN N <purupaul3@gmail.com> wrote:
> Dear all,
>
> Greetings.
>
> Please inform me PTC(Production test coupon requirement) for below
> details--
>
> Construction Code : ASME SEC III DIV 1 NB
>
> Shell Material : IS 2062 E 250 B
>
> MDMT : 0 Deg Celcius
>
> PLATE THICKNESS: 6mm
>
> For 6mm Plate, Production test coupon is required?
>
> Regards
> N.Purushothaman
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
>
--
Thanks & Regards
Krishna Mudhale
Mob.:+91-8796076925/ 9860459776
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
As per ASME Sec.VIII Div.1, PTC is required only when the subject
material is not exempted from impact requirement. Refer clause
UG-84(i) for more clarification about PTC requirement.
On 7/3/14, PURUSHOTHAMAN N <purupaul3@gmail.com> wrote:
> Dear all,
>
> Greetings.
>
> Please inform me PTC(Production test coupon requirement) for below
> details--
>
> Construction Code : ASME SEC III DIV 1 NB
>
> Shell Material : IS 2062 E 250 B
>
> MDMT : 0 Deg Celcius
>
> PLATE THICKNESS: 6mm
>
> For 6mm Plate, Production test coupon is required?
>
> Regards
> N.Purushothaman
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
>
--
Thanks & Regards
Krishna Mudhale
Mob.:+91-8796076925/ 9860459776
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments